An oil composition which has a kinematic viscosity at 100 °C of from 32 to 50 cSt and which contains less than 3%. Polynuclear aromatic
compounds is employed as a process oil for rubber compounds, especially aromatic rubbers. The process oil is compatible with aromatic rubbers.
Specification | Heavy RPO | Light RPO |
---|---|---|
V 100°C | 35 min | 35 max |
Density @ 15°C (Kg/cm3) | 1.050 | 1.010 |
Flash Point (°C) | 200-230 | 200-230 |
RI at 70°C | 1.5600 | 1.5500 |